evanhall - posted 19:55, Wednesday 05 February 2025 - last comment - 14:42, Wednesday 26 February 2025(11884)
Continued prism coupling experiments with copper leaf

Swadha, Evan

We continued coupling experiments between two prisms with copper leaf and achieved transmission as high as 3%.

We are still not happy with our procedure, but it is as follows (with critique):

  1. Blow the prism surfaces clean with compressed air. Then drag wipe with isopropanol. This removes copper specks large enough to be seen with the eye, but it is unclear to what extent copper remains pressed onto the surface from previous coupling attempts.
  2. The drag wiping seems to remove surface charge from the glass, which is actually disadvantageous because we like the leaf to stick to the glass when placed there. We found that cellophane tape applied to (and then removed from) the surface restored the charge. We might like to find a similar material that does not involve adhesive.
  3. We cut two strips of copper leaf about 5 mm × 25 mm. We use a PTFE-coated razor blade to press into the leaf, which is placed on top of UHV foil. We also tried placing the leaf on nylon to try to preserve the blade a bit longer, but this may charge the copper so we have put it aside for now.
  4. Using tweezers, we transfer each strip to either side of the clear aperture of one of the prism faces. Throughout the entire process with the leaf, the HVAC in the flow bench and clean room is off because air currents are too powerful.
  5. Each prism is on a separate mount. We press the two mounts together so the prism faces contact. This is currently a bit of a messy process and it may be the case that we are causing the leaf to wrinkle, although it looks reasonably flat after pressing.
  6. One of the mounts is kinematic and we can see optical fringes under bright illumination at the interface. Twisting the kinematic screws to increase the interface compression will increase transmission to a point, but continuing to twist eventually decreases coupling for some reason I do not yet understand.
Comments related to this report
evanhall - 14:36, Friday 14 February 2025 (11889)

We improved this procedure through the following:

  • On Sławek's advice, we used an alpha wipe (100% polyester) to charge the outward portions of the prism faces, rather than cellophane tape. This seems to have worked well. We may still need cellophane tape to remove bits of shredded copper between tests.
  • We found that strips of copper were too easily ripped or shredded due to shear at the interface as we were tightening down the contact between the faces and the copper. We switched to using three small (~3 mm diameter) pieces of copper leaf. This gave a better transmissivity result (see below) and also enabled us to keep the blowers on during the whole procedure.

Our procedure to prepare the faces between tests is:

  • Cellophane tape is applied to remove shredded pieces of leaf (we are worried that drag wiping at this stage may scratch the glass).
  • The prism faces are drag wiped with acetone (to dissolve the acrylic of the cellophane adhesive). The acetone is not allowed to dry; the wipe is finished with DI water to avoid precipitation of anything in the acetone.
  • The outward portions of the prism faces are gently brushed with an alpha wipe to charge the faces.
  • The copper leaf is kept under a weighted piece of UHV foil so that it does not blow around. A piece of copper is ripped off from the square leaf with tweezers and then stuck to one of the two prism faces. This is repeated twice to get three bits of copper on one of the faces.

After this procedure, we were able to get coupling in excess of 30% in the p polarization. We mounted the two prism stages on a rotating optical breadboard and took transmission readings as a function of angle of incidence. An MCMC analysis of the data suggests the gap size is 1.5 µm, which is still larger than the 600 nm of the leaf itself (measured with a micrometer). The MCMC determines the index of refraction to be 1.43, which is lower than the 1.445 expected for Corning 7980, but the constraint is not too tight and is also susceptible to any difference in power efficiency of the reflection and transmission photodiodes, which we did not set up too carefully. In contrast, the gap size is determined by the falloff in transmission with angle of incidence, which is well-calibrated.

Non-image files attached to this comment
evanhall - 10:30, Tuesday 18 February 2025 (11891)

There is a question of why, if the copper leaf is supposedly 600 nm as measured by micrometer, the gap size here appears to be about 1.5 µm.

I hypothesized that it might be due to insufficient pressure applied from way the prisms were clamped (each on a platform with a clamping arm, as you might do for a PBS). The clamping arm provides a restoring shear via its nylon-tipped setscrew.

I replaced this clamping geometry with three angle brackets for each prism, with 8-32 tapped through-holes that can accommodate setscrews. I repeated the contacting procedure described above and was not able to significantly raise the transmission higher than the values previously reported (0.3 to 0.4 in power at best). I did not take detailed data as a function of angle, but it seems this altered clamping geometry did not attain an appreciably smaller gap size.

It is also worth remarking that both clamping geometries don't really provide proper kinematic contact; the point of this two-platform geometry was to bring the prisms nearly into contact in some controlled (perhaps interferometric) fashion, rather than relying on actual contact via a spacer material (leaf in this case).

evanhall - 14:42, Wednesday 26 February 2025 (11900)

Swadha, Adam, Evan

We turned the entire coupling setup vertical so that we could let gravity maintain an approximately kinematic contact.

Simplify placing the upper prism on the spots of leaf results in a coupling of a few ppm or less, so presumably many microns of gap size. We suspect the leaf is wrinkled in some way when cut and/or placed, although we have taken some care to avoid obvious folds or scrunches when we place it.

Applying pressure at the interface seems to bring the gap size down to what we saw previously, probably 1–2 µm as inferred from the 30% or so transmission in p. (We have some transmission vs. angle data that we have not analyzed yet.)

This setup has the nice feature that when the flow bench lights are on, they produce obvious fringing at the interface, so it is possible to see the parallelism of the faces down to the level of a few fringes.