Jasper, Nikhil, Wen
We spent some time on Thursday to fix the dichroic filtering of the pump in the squeezed vacuum path. The pump power was noticably high on the pump reflection path because I put a dual superpolished HR mirror temporarily for rough alignment. We replaced it with a superpolished dichroic optics, but there's still fair amount of green (25 uW) coming out of chamber.
To resolve this problem, we did some testing on the superpolished dichroics available to us. This was done on the sqz table right after SHG. We tried three different AOIs (roughly) and measured the reflected power with 60 mW input power.
| 22.5 deg | 45 deg | 67.5 deg | |
| Dichroic E1600367 | 17 mW | 1.2 mW | 17 mW |
| Dichroic E0900491 | 2.2 mW | 1.1 mW | 12 mW |
At the optimal AOI of 45 deg, the dichroic has a power transmission of >95%. However, the transmission reduced to ~70% at angles of 22.5 deg or 67.5 deg.
We also tested the optics to make sure which side has the HR coating for 1064. The power reflectivity for 1064 was measured to be >99% for all dichroics (<1% loss).
For the pump in VOPO chamber, the power was measured at the VOPO REFL (4.8 mW), after 1st dichroic (50 uW), and after 2nd dichroic (25 uW). The low transmission of pump on the 2nd dichroic is very likely to be the AOI, although its pretty close to 45 deg. We will need to move the optics a bit to find the optimal output path.